ASTM A395_A395M-99(2022) - 道客巴巴
2024年11月6日 · Published October 2022. Originallyapproved in 1955. Last previous edition approved in 2018 as A395/A395M – 99(2018). DOI: 10.1520/A0395_A0395M-99R22.2 For referenced ASTM standards, visit the ASTM website, www.astm.org, orcontact ASTM Customer Service at [email protected].
Designation: A395/A395M − 99 (Reapproved 2018) Standard Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures1 This standard is issued under the fixed designationA395/A395M; the number immediately following the designation indicates the year
ASTM A395 高温承压铁素体球铁技术规范 - 道客巴巴
2019年3月26日 · astm标号:a395/a395m-99高温承压铁素体球铁技术规范标准 1.范围 1.1此技术规范适用于高温承压球铁铸件。在温度不超过450°f条件下,所有等级铸件都适合;在温 度超过450°f、不超过650°f条件下,只有60?40?18级铸件适合(注1)。 1.
A395/A395M Standard Specification for Ferritic Ductile Iron …
2022年10月10日 · Standard Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures. This specification covers standard requirements for ductile iron castings for pressure-retaining parts for use at elevated temperatures. Castings are classified by grades based on mechanical property requirements.
This standard is issued under the fixed designation A395/A395M; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval.
A395 vs A216: What's the Difference? - MFG Shop
2024年12月5日 · When comparing the mechanical properties of A395 and A216, A395 ductile iron exhibits higher ductility and better wear and impact resistance compared to A216 carbon steel. A395 has a tensile strength ranging from 60,000 to 100,000 psi and a yield strength of at least 40,000 psi, with elongation at break between 18% and 30%.
(正版标准) ASTM A395 -1999(R2018) - 道客巴巴
2019年1月3日 · Scope1.1 This specif i cation covers ductile iron castings forpressure-retaining parts for use at elevated temperatures. Cast-ings of all grades are suitable for use up to 450 °F.
a395是什么材质 - 百度知道
A395 是球墨铸件,其综合性能接近于钢,正是基于其优异的性能,已成功地用于铸造一些受力复杂,强度、韧性、耐磨性要求较高的零件。 球墨铸铁 已迅速发展为仅次于灰铸铁的、应用十分广泛的铸铁材料。 A395是含碳量大于2.11%的 铁碳合金,由工业生铁、废钢等钢铁及其 合金材料 经过高温熔融和铸造成型而得到,除Fe外,还含及其它铸铁中的碳以石墨形态析出,若析出的石墨呈条片状时的铸铁叫灰口铸铁或灰铸铁、呈蠕虫状时的铸铁叫蠕墨铸铁、呈团絮状时的铸铁叫白 …
ASTM A395 Properties⚙️ (Chem., Mech. & Rankings) rev. 2022
2020年9月15日 · ASTM A395 is a Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures. Category Wrought Iron, Cast Iron, and Malleable Iron
ASTM A395/A395M-99(2004) 用于高温的铁素体球墨铸铁压铸件的 …
5 天之前 · ASTM A395/A395M-99(2004) 用于高温的铁素体球墨铸铁压铸件的标准规范 Standard Specification for Ferritic Ductile Iron Pressure-Retaining Castings for Use at Elevated Temperatures