which material is good with ferric chloride? - Eng-Tips
2005年11月1日 · As a manufacturer of ferric chloride who frequently trials the material at WTPs and WWTPs, we recommend that no metal (except for titanium and possibly Hastelloy-C) be …
Chloride Limit for Zirconium and Titanium - Eng-Tips
I am looking for the chloride limit of both zirconium and titanium. We are beginning the switch from chlorine gas to bleach for the treatment of our cooling tower water and want to avoid any …
Chloride Limit for Zirconium and Titanium - Chemical process ...
I am looking for the chloride limit of both zirconium and titanium. We are beginning the switch from chlorine gas to bleach for the treatment of our cooling tower water and want to avoid any …
Allowable Chlorides in Cooling Tower Circulating Water 3 - Eng-Tips
2002年10月14日 · Cooling Tower suppliers nominate an allowable chloride level of approx. 750ppm (50C, pH=6-8) for circulating water. Corrosion resistance tables nominate a chloride …
Chloride corrosion pitting on SS316 - Corrosion engineering - Eng …
2020年4月26日 · I don't think 2205 is a standard material for plate and frame heat exchangers. 254 and Ti are the chloride resistant alloys available from a leading manufacturer. Titanium is …
Tank/Relief Design: Air Surge from Tanker Off-loading
2019年5月1日 · 2. The current tank to be replaced is bottom entry. Iron chloride has a tendency to foam, and I am concerned that the relief of the 700-1000 SCFM (my initial swag, not detailed …
HCL ACID AND STAINLESS STEEL TANKS - Eng-Tips
2005年8月17日 · Hi, I am a bit concerned. My engineers are builing a Stainless steel (316) tank to hold highly concerntrated HCL acid. I believe we would be best to use other material as the …
C02 Generation methods/Titanium Dioxide Catalyst fact/fiction 1
2008年5月14日 · Honestly, I'm not a chemical engineer so much of the discussion was outside of my experience- I wasn't able to derive a clear answer about the effectiveness of using …
6AL4V Titanium stress relief? - Metal and Metallurgy engineering
2016年8月18日 · Creep flattening consists of heating titanium sheet between two clean, flat sheets of steel in a furnace containing an oxidizing or inert atmosphere. Vacuum creep …
Cadmium plated hardware used on Titanium parts... 10 - Eng-Tips
2009年7月10日 · Titanium is embrittled by cadmium from room temperature (solid Cd) up to the 320 C (molten Cd). This includes alloys such as Ti-6Al-4V, Ti-13V-11Cr-3Al, and Ti-8Al-1Mo …